Skip to main content
. 2022 Nov 12;14(22):4878. doi: 10.3390/polym14224878

Table 4.

Mechanical characteristics of the neat and weathered Hmi/PHB materials (90 days of exposure).

Content of Hmi
%
Exposure Time
Days
Tensile Strength
(Mean ± SD = 0.05, n = 10) MPa
Elongation at Break
(Mean ± SD = 0.2, n = 10)
%
5 0 5.5 6.1
5 90 1.9 4.5
0 0 1.7 3.6
0 90 2.7 4.2