Skip to main content
. 2022 Nov 15;15(22):8063. doi: 10.3390/ma15228063

Figure 3.

Figure 3

(a) LIFT of HEA film. (b) SEM images of single sub-1 μm particles of CoCrFeNiMo0.2 transferred on a cover glass at different fluences per pulse (J/cm2/pulse) under NA=0.26 focusing. Laser irradiation: 230 fs, 515 nm. Thickness of HEA was 50 nm.