. 2022 Nov 17;14(22):4976. doi: 10.3390/polym14224976

Figure 2.

Figure 2

Contact angles of water (θW) and diiodomethane (θD) on films made of PLA, Mg particles and CTAB for non-degraded and degraded samples for 1 and 3 months. (a) Non-containing magnesium films; (b) magnesium-containing films. The texture of θD is included to differentiate more clearly between cases in which θD > θW. All data are given as mean and standard deviation.