Skip to main content
. 2022 Dec 3;33(12):78. doi: 10.1007/s10856-022-06700-4

Fig. 9.

Fig. 9

Schematic diagram of the procedure for the preparation of PCL/PNIPAAm nucleus-sheath smart nanofibers containing NK (A). The release profile of NK from PCL/PNIPAM/NK nanofibers (B). Measurement of adhesion and water contact angle of purified platelets on nanofibers (C). Where a, d for PCL/PNIPAAm nanofibers; b, e for PCL/PNIPAAm/NK (5/5/1) nanofibers; c, f for PCL/PNIPAAm/NK (5/5/2) nanofibers. a–c for temperature 32 °C, d-f for temperature 25 °C [136]