Skip to main content
. Author manuscript; available in PMC: 2023 Apr 19.
Published in final edited form as: ACS Macro Lett. 2022 Mar 21;11(4):460–467. doi: 10.1021/acsmacrolett.2c00053

Figure 3.

Figure 3.

SEC traces with differential refractive index detection of a representative sequential ROMP polymer (BB-E45, 20-b-BB-P15, 10). The macromonomer traces are included for reference. From the multi-angle light scattering detector and a Zimm analysis, the BB-PPO aliquot has a Mw = 11,600 g/mol and Đ = 1.20 and the BB-diblock has a Mw = 55,300 g/mol and Đ = 1.10, both were within error of the targeted molecular weight. The small peak at ~17 minutes in the BB-PPO chromatogram is likely a small molecule impurity in the PPO macromonomer, possibly 18-crown-6 ether, that does not impact the subsequent polymerization