Skip to main content
. 2022 Nov 30;15(23):8543. doi: 10.3390/ma15238543

Figure 6.

Figure 6

OM micrographs of the corrosion pits edges—S specimen after 24 h exposure in 1 M Cl solution (represented by 5 wt % FeCl3 solution), cross section: (a) 20 ± 3 °C, magnification 100×; (b) 20 ± 3 °C, magnification 400×; (c) 50 °C, magnification 100×; (d) 50 °C, magnification 400×.