Skip to main content
. 2022 Nov 30;15(23):8543. doi: 10.3390/ma15238543

Figure 8.

Figure 8

SEM micrograph—detail of the corrosion pit edge. S specimen after 24 h exposure at 20 ± 3 °C, surface area, oxalic acid electroetched (ASTM A262 practice A), 1000× magnification.