Table 1. Properties of the Samples of CdSe QDs with ZnS Shell47 Used in Case Study I and CdSe QDs with ZnS/CdS/ZnS Multicomponent Shell48 Used in Case Study I and Case Study III.
| sample | core [diameter (nm)] | shell [thickness (MLs)] | medium | concentration |
|---|---|---|---|---|
| CdSe/ZnS QD solution | CdSe [2.3] | ZnS [1] | hexane | <10–6 M |
| CdSe/ZnS QD solution | ZnS [3] | hexane | <10–6 M | |
| CdSe/ZnS QD solution | ZnS [5] | hexane | <10–6 M | |
| CdSe/ZnS/CdS/ZnS QD solution | ZnS/CdS/ZnS [1/1/1] | hexane | <10–6 M | |
| single CdSe[ZnS/CdS/ZnS] QD in PMMA | PMMA | <1 μm–2 |