Table 2.
Metals | Types of plastics | pH | size | Temperature (℃) |
Qm (μg/g) |
References |
---|---|---|---|---|---|---|
Pb(Ⅱ) | Pristine DFM | 6.0 | 175 × 95 mma | 25 | 265.63 | This work |
Aged DFM | 6.0 | 175 × 95 mma | 25 | 384.16 | ||
Pristine PS | NMb | 0.1 μm | 25 ± 2 | 160.00 | [40] | |
Aged PS | NMb | 0.1 μm | 25 ± 2 | 202.00 | ||
Pristine PVC | 6.5 | 280 μm | 25 | 2518 ± 125 | [49] | |
Beached PE | NMb | NMb | 20 ± 1 | 0.72 | [67] | |
Pristine PE | 6.5 | ∼ 4 mm | 25 | 0.19 | [68] | |
Beached PE | 6.5 | ∼ 4 mm | 25 | 2.74 | ||
Pristine PET | 6.3 | < 5 mm | NMb | 4930.00 | [69] | |
Pristine PP | 6.3 | < 5 mm | NMb | 5550.00 | ||
Cd(Ⅱ) | Pristine DFM | 6.0 | 175 × 95 mma | 25 | 79.75 | This work |
Aged DFM | 6.0 | 175 × 95 mma | 25 | 105.32 | ||
Pristine PS | NMb | 0.1 μm | 25 ± 2 | 105.00 | [40] | |
Aged PS | NMb | 0.1 μm | 25 ± 2 | 175.00 | ||
Pristine PS | 4.0 | NMb | 25 | 20.15 | [70] | |
Pristine PP | NMb | 74 μm | 25 | 36.10 | [71] | |
Pristine PVC | 6.5 | 280 μm | 25 | 1748 ± 505 | [49] | |
Beached PE | NMb | NMb | 20 ± 1 | 0.01 | [67] | |
Pristine PE | 6.5 | ∼ 4 mm | 25 | 0.01 | [68] | |
Beached PE | 6.5 | ∼ 4 mm | 25 | 0.25 | ||
Pristine PET | 6.0 | 75 μm | 24 ± 1 | 250 ± 10 | [27] | |
Pristine PVC | 6.5 | 280 μm | 25 | 1748 ± 505 | [49] | |
Sr(Ⅱ) | Pristine DFM | 6.0 | 175 × 95 mma | 25 | 58.54 | This work |
Aged DFM | 6.0 | 175 × 95 mma | 25 | 64.34 | ||
Pristine PP | NMb | 100–150 mm | 25 | 68 ± 12.6 | [72] | |
Pristine PET | NMb | 100–150 mm | 25 | 360 ± 79.2 | [29] | |
Pristine PE | NMb | 100–150 mm | 25 | 470 ± 106 | ||
Pristine PVC | NMb | 100–150 mm | 25 | 790 ± 238 |
Note: 175 × 95 mma (A whole DFM); NMb (Not Mentioned); Abbreviations: PP (Polypropylene); PET (Polypropylene Terephthalate); PS (Polystyrene); PVC (Polyvinyl Chloride); PE (Polyethylene).