Table 3. TG and DTG Data of PET and PET Composites in N2 at a Heating Rate of 10 °C min–1.
| samples | T5% (°C) | Tmax (°C) | Rmax (% min–1) | Cw (%) |
|---|---|---|---|---|
| PET | 401.51 | 439.71 | 21.06 | 16.97 |
| FRPET | 400.27 | 445.36 | 19.20 | 18.16 |
| 3%DOPO-POSS/FRPET | 402.20 | 443.24 | 18.41 | 19.82 |
| 5%DOPO-POSS/FRPET | 401.30 | 439.22 | 18.35 | 20.68 |
| 7%DOPO-POSS/FRPET | 402.03 | 437.36 | 18.92 | 23.70 |
| 9%DOPO-POSS/FRPET | 399.53 | 436.97 | 17.24 | 23.56 |