Skip to main content
. 2022 Dec 19;19(24):17063. doi: 10.3390/ijerph192417063

Table 4.

Environmental risk assessments for pollution by PTMs in leaching solutions (bold values are single-factor contamination indexes).

PTM Cd Cr Cu Mn Ni WQI Result
Sintered slag Static soaking -- 0.720 0.022 1.600 0.430 67.078 Good
Dynamic leaching 0.400 0.760 0.177 19.300 8.300 616.411 Undrinkable
Waste slag Static soaking -- 0.800 0.821 3.860 8.700 186.900 Poor