. 2022 Dec 17;15(24):9025. doi: 10.3390/ma15249025

Figure 4.

Figure 4

(a) SEM graph of Ce, Pr:LuAG ceramic after thermal etched at 1500 °C for 3 h in air with a slightly flowing O2; (b) grain size distribution; (ce) element analysis of position 1 and position 2 of the triple grain boundary junctions by EDS, respectively.