Young’s modulus and elongation at break % of non-irradiated and gamma-irradiated PLA:PCL electrospun scaffolds

Sample Young’s modulus (MPa) Elongation at break %
Non-irradiated scaffolds 0.33 ± 0.03 200 ± 12.5