Skip to main content
. 2022 Dec 16;22(24):10176–10183. doi: 10.1021/acs.nanolett.2c04216

Figure 1.

Figure 1

(a) Schematic of the TSE separator fabrication process with (b) pictures of the TSE separator showing a 9 × 6 cm2 area (left) with a thickness of 47 μm (center) and demonstrating its flexibility (right). Results of material characterization of prepared TSEs with 3, 5, and 10 wt % XNBR binder (TSE-X3, TSE-X5, TSE-X10, respectively) using (c) FT-IR spectroscopy, (d) Raman spectroscopy, and (e) XRD. (f) Results of testing the Young’s modulus by compression and ionic conductivity by EIS.