Skip to main content
. 2023 Jan 3;24(1):869. doi: 10.3390/ijms24010869

Figure 8.

Figure 8

Evaluation of the survival of P. aeruginosa on uncoated samples (a), on PTFE without NPs (b), and on the composite coating of fluoroplast/NP Ag2O 0.1% (c). Living cells are colored green, dead cells red. Magnification ×400.