Figure 3.

Figure 3

DSC thermograms of (a) neat epoxy, (b) 0.25phr DMA-4CNBR/EP, (c) 0.5phr DMA-4CNBR/EP, (d) 0.75phr DMA-4CNBR/EP, and (e) 1phr DMA-4CNBR/EP, at different heating rates. (f) The correlation fitting curves of different content DMA-4CNBR modified epoxy resin systems based on Kissinger’s theories.