Skip to main content
. 2022 Dec 22;24(1):502–514. doi: 10.1021/acs.biomac.2c01418

Table 2. Flow Behavior of Each Ink Formulation: Viscosity, Shear-Thinning Coefficients, Yield Stress, and Recovery Rate during the Extrusion.

compositions n viscosity [Pa·s] K τ0 [Pa] recovery rate [%]
GelMA30 0.82 1.22 0.01 0.04  
GelMA60 0.41 4.62 0.73 0.07  
GelMA30GA 0.28 4.05 0.43 0.08  
GelMA60GA 0.92 0.05 0.01 0.02  
GelMA30GA-2.5Fe 0.42 76 0.80 0.74  
GelMA60GA-2.5Fe 0.26 4.16 0.16 0.04  
GelMA30GA-5Fe 0.03 7940 276 83 ∼73
GelMA60GA-5Fe 0.23 6371 21 21 ∼72