(A) Probing Li+ ion diffusion
during niobium–tungsten
particle charging. Schematic of the optical setup used to probe operando the cell voltage charge ion due to migration, leading
to particle cracking. The fracture propagation can be observed due
to optical scattering images at 283 s from the beginning of polarization.
Reprinted by permission from Macmillan Publishers Ltd.: Nature Materials,
Merryweather, A. J.; Jacquet, Q.; Emge, S. P.; Schnedermann, C.; Rao,
A.; Gray, C. P. Nat. Mater.2022, 21 (11), 1306–1313 (ref (383)). Copyright 2022. (B) Correlative multimicroscopy
approach coupled with machine vision algorithm for probing the electrodeposition
of Ni-based NPs. Reproduced from Bridging the Gap between Single Nanoparticle
Imaging and Global Electrochemical Response by Correlative Microscopy
Assisted By Machine Vision, Godeffroy, L.; Lemineur, J. F.; Shkirskiy,
V.; Miranda Vieira, M.; Noel, J. M.; Kanoufi, F. Small Methods, Vol. 6, Issue 9 (ref (356)). Copyright 2022 Wiley.