Skip to main content
. 2021 Jul 1;1(1):6–10. doi: 10.1021/acsmeasuresciau.1c00006

Figure 3.

Figure 3

(a) Image of quantified surface charge in the same area of the CF UME as the electrochemical maps in Figure 2. Scale bar: 1.2 μm. (b) Correlation between Isub and local surface charge at the CF UME surface.