Skip to main content
. 2022 Dec 26;10:rbac107. doi: 10.1093/rb/rbac107

Figure 1.

Figure 1.

(a) Schematic illustration of the fabrication of PC/collagen by LBL process. (b) The shifts of ΔF and ΔD monitored by QCM-D during fabricating (PC/collagen)6 at pH 8.5. (c) The thickness of PC/collagen multilayers deposited onto QCM-D sensor at pH 8.5.