Fig. 8. Controlled experiment of catalytic degradation of MOr at (A) NaBH4, MOr, and Ag/Ni-P(NMA-MAa) [conditions: [MOr] = 0.080 mM, [NaBH4] = 9.65 mM, Ag/Ni-P(NMA-MAa) = 85.71 μg mL−1], (B) MOr, NaBH4 and P(NMA-MAa) [conditions: [MOr] = 0.080 mM, P(NMA-MAa) = 9.65 μg mL−1, [NaBH4] = 9.65 mM] (C) MOr and NaBH4 [conditions: [MOr] = 0.080 mM, [NaBH4] = 9.65 mM, without addition of P(NMA-MAa) and Ag/Ni-P(NMA-MAa)], (D) MOr and Ag/Ni-P(NM) [conditions: [MOr] = 0.080 mM, Ag/Ni-P(NMA-MAa) = 85.71 μg mL−1, in the absence of NaBH4].