TABLE 1.
Temperature of maximum weight loss rate (Tp) and residual carbon rate (RC) of the starch composite films.
| Sample | Tp (°C) | RC (%) | Sample | Tp (°C) | RC (%) |
|---|---|---|---|---|---|
| CS | 315.5 | 5.2 | CA | 322.9 | 9.5 |
| CS/CMC-0.2 g | 307.1 | 18.5 | CA/CMC-0.2 g | 306.2 | 20.1 |
| CS/CMC-0.4 g | 305.0 | 22.5 | CA/CMC-0.4 g | 304.1 | 21.3 |
| CS/CMC-0.6 g | 296.1 | 16.3 | CA/CMC-0.6 g | 301.1 | 18.8 |
| CS/CMC-0.8 g | 295.2 | 22.9 | CA/CMC-0.8 g | 298.2 | 13.3 |
| CS/CMC-1.0 g | 293.2 | 22.1 | CA/CMC-1.0 g | 295.2 | 9.5 |