Skip to main content
. 2023 Jan 4;24(2):903. doi: 10.3390/ijms24020903

Table 1.

Characteristics of the LNPs used in this study.

LNP Type Diameters (nm) Polydispersity Index (PdI) ζ-Potential (mV) Recovery Rate (%)
DOPE/SM-LNP 102 ± 6.6 0.21 ± 0.06 −5.36 ± 2.4
R8-MITO-Porter 97.6 ± 5.9 0.26 ± 0.02 29.5 ± 3.7
R8-MITO-Porter (BBR) 93.6 ± 1.6 0.28 ± 0.01 30.1 ± 4.8 12.2 ± 4.6