Skip to main content
. 2023 Jan 8;24(2):1230. doi: 10.3390/ijms24021230

Figure 4.

Figure 4

Figure 4

(A) Hydrogel CMC-E3, (B) Hydrogel HEC-E3, (C) Hydrogel CMC-E5 and swelling percentage of the hydrogels (D) at 25 °C for 24 h, and (E) at 35 °C for 24 h; (F) FTIR spectra of CMC-E3 hydrogel, CMC and cellulose powder; scanning electron microscopic images of hydrogels (G) CMC-E3, (H) HEC-E3 and (I) CMC-E5.