Table 3.

Hardness and stereological parameters of carbides in the microstructure of investigated alloys.

Alloy Condition Hardness
HV
Stereological Parameters of Carbides
AA (%) A (μm2) ξ
Ti-0.2C Casting 204 ± 6 1.51 10.45 0.62
Homogenization 230 ± 4 1.20 8.98 0.68
Hot rolling 191 ± 7 1.36 16.21 0.93
Recrystallization annealing 205 ± 4 1.16 16.46 0.94
Solution treatment 212 ± 4 0.42 5.65 0.92
Solution treatment and aging 244 ± 6 1.08 4.25 0.90

AA—area fraction; A—mean area; ξ—shape factor.