Skip to main content
. 2023 Jan 30;28(3):1321. doi: 10.3390/molecules28031321

Figure 3.

Figure 3

Before hydrogel formation (a). After hydrogel formation (b). Temperature (T) sweep experiment at t = 25–65 °C of C-OSSPG0.2/BP hydrogel (c). FT-IR spectra of PVA, borax, BP and C-OSSPG0.2/BP hydrogel (d). The SEM image of BP and C-OSSPG0.2/BP (e). The relevant physical properties of the C-OSSPG0.2/BP hydrogel (f).