Skip to main content
. 2023 Feb 5;39(6):2135–2151. doi: 10.1021/acs.langmuir.2c02715

Figure 5.

Figure 5

XRR curves and the corresponding SLD profiles of Au NP films transferred onto H-terminated Si at three different surface pressures recorded (a) 2 months and (b) 12 months after the deposition. Reprinted with permission from ref (53). Copyright 2014 AIP Publishing.