Figure 2

The UV–VIS absorption spectra of freshly and three months post synthesized Cit-Au NPs and Ga-Au NPs (A), hydrodynamic size distribution for Cit-AuNPs and Ga-AuNPs (B), Zeta potential spectra of Cit-Au NPs and Ga-Au NPs at acidic 5.6pH (C,E respectively), and Zeta potential spectra of Cit-Au NPs and Ga-Au NPs at normal physiological 7 pH (D,F respectively).