. 2023 Jan 19;13(2):203. doi: 10.3390/biom13020203

Figure 4.

Figure 4

Photos of nanofibrous mats prepared by electrospinning, on the top, of 160% (w/v) solutions in DMF, in W/A, and DMAc (using 15 kV voltage, 0.1 mL/h of flow rate, and 15 cm) and, on the bottom, the associated SEM images.