Skip to main content
. 2022 Apr 11;2(4):275–286. doi: 10.1021/acspolymersau.2c00005

Figure 4.

Figure 4

Responses of P3KnT to water sorption at increasing RH. (a) DVS curves for P3KnT bulk powders. (b) Change in thin film thickness as measured by ellipsometry. Values for change in thickness at 95% RH are extrapolated from best fit curves from 25% to 90% RH.