Skip to main content
. 2023 Jan 20;9(2):93. doi: 10.3390/gels9020093

Table 4.

Values of power law model parameters (ηa,50, K, and n) of raw and agglomerated PPSPs with different concentrations of MD binder.

Sample MD
Concentration
(%)
ηa,50 (Pa·s) K (Pa·sn) n
Raw PPSP   1.47 ± 0.02 c 4.78 ± 0.17 ab 0.70 ± 0.01 d
Agglomerated
PPSP
0 (control) 1.67 ± 0.02 a 4.89 ± 0.01 a 0.73 ± 0.00 c
10 1.58 ± 0.06 b 4.70 ± 0.02 b 0.72 ± 0.01 c
20 1.10 ± 0.02 d 3.18 ± 0.10 c 0.73 ± 0.00 c
30 0.76 ± 0.01 e 1.45 ± 0.07 d 0.77 ± 0.00 b
40 0.59 ± 0.00 f 1.33 ± 0.07 d 0.79 ± 0.01 a

Each value is the mean of triplicate measurements ± SD. Means with different lowercase letters (a–f) within each column are significantly different (p < 0.05).