Table 5.

Values of dynamic rheological parameters (G′, G″, and tan δ) of raw and agglomerated PPSPs with different concentrations of MD binder.

Sample MD
Concentration
(%)
G′ (Pa) G″ (Pa) tan δ
Raw PPSP   6.71 ± 0.05 c 12.1 ± 0.01 c 1.80 ± 0.02 d
Agglomerated
PPSP
0 (control) 8.13 ± 0.03 b 14.3 ± 0.08 b 1.76 ± 0.00 e
10 8.68 ± 0.04 a 15.8 ± 0.03 a 1.82 ± 0.01 d
20 5.48 ± 0.03 d 11.1 ± 0.06 d 2.02 ± 0.00 c
30 2.27 ± 0.04 e 6.15 ± 0.04 e 2.71 ± 0.04 b
40 1.86 ± 0.03 f 5.70 ± 0.08 f 3.07 ± 0.03 a

Each value is the mean of triplicate measurements ± SD. Means with different lowercase letters (a–f) within each column are significantly different (p < 0.05).