Raman shift of the as-deposited Mo, i.e., without post laser treatment showing the Mo deposited on the surface (this process is in vacuum and metallic Mo is expected); post deposition laser treated with 1.5 and 0.2 W showing the formation of oxides MoOx on the surface of the Mo-coated sample (this process is in air, and oxidation is expected).