Table 1.
Laser Parameter | Value |
---|---|
Nano-Structuring | |
Fluence range | 5–15 J/cm2 |
Frequency | 50 kHz |
Scanning speed | 20 mm/s |
Pulse duration | 40 fs |
Step size | 100 µm |
Beam wavelength | 1030 nm |
Coating and post treatment | |
Fluence | 3 J/cm2 for deposition process, 1.5, and 0.25 J/cm2 for post-deposition treatment |
Frequency | 150 kHz for deposition and 50 kHz for post-deposition treatment |
Scanning speed | 3325 mm/s for post-deposition treatment |
Pulse duration | 240 fs for deposition process and 40 fs for post-deposition treatment |
Step size | 10 µm for post-deposition treatment |
Beam wavelength | 1030 nm |