Skip to main content
. 2023 Feb 4;15(4):788. doi: 10.3390/polym15040788

Figure 20.

Figure 20

Maximum load for single lap joint tests for joints with PBT-GF30 substrates as a function of the adhesive thickness, dry and after aging at 70 °C for two months.