Reflection loss values that measured and details of different samples.
Sample | Nanocomposite | Amount of polymer (wt%) | Resin wt% | Thickness (mm) | RL (dB) |
---|---|---|---|---|---|
1 (single-layer) | Fe3O4/HNTs-60% PS | 60 | 60 | 3 | −5.07 |
2 (bilayer) | 60 | 85 | −11.74 | ||
3 (bilayer) | 60 | 90 | −9.71 | ||
4 (single-layer) | 60 | 60 | 4 | −6.88 | |
5 (bilayer) | 60 | 85 | −26.9 | ||
6 (bilayer) | 60 | 90 | −10.72 | ||
7 (bilayer) | Fe3O4/HNTs-72% PS | 72 | 85 | 3 | −7.05 |
8 (bilayer) | 72 | 85 | 4 | −7.4 | |
Pure resin | — | 0 | 100 | 3 | −1.7 |