Skip to main content
. Author manuscript; available in PMC: 2011 May 17.
Published in final edited form as: Materials (Basel). 2011 May;4(5):857–867. doi: 10.3390/ma4050857

Figure 7.

Figure 7

SEM images showing extent of circumferential cracking on (a) NCD with 60 kg and 100 kg loads, and 100 kg loads of (b) NCD; (c) M1; (d) M4; (e) M3; and (f) M2.