Characterization measurements of tested groups.

Scaffolds Filament width (μm) Pore size (μm) Contact angle° Porosity (%) Density (g/cm3) Cell viability %
PCL 326 ± 20.8 347 ± 22.55 94 ± 10.44 56 ± 3.7 0.24 ± 0.016 83.27 ± 5.55
1 wt% GO-PCL 332 ± 21.66 339 ± 22.72 87 ± 9.67 52 ± 3.5 0.26 ± 0.017 86.34 ± 5.76
3 wt% GO-PCL 335 ± 21.36 335 ± 20.01 83 ± 9.22 50 ± 3.3 0.27 ± 0.018 79.36 ± 5.29