Skip to main content
. 2024 Oct 10;29(20):4798. doi: 10.3390/molecules29204798

Table 1.

DSC melting temperatures (Tm), crystallization temperature (Tc), and degree of crystallinity (Xc) with standard deviations of PP films with 0.5 and 2 wt% additives.

Films Tm (°C) Tc (°C) ΔHm (J/g) Xc (%)
PP BLK 162.79 ± 0.01 120.85 ± 0.25 77.88 ± 0.33 37.26 ± 0.16
0.5 wt% GN 161.76 ± 0.17 119.77 ± 0.02 88.89 ± 1.30 44.77 ± 0.65
0.5 wt% BIOC 162.92 ± 0.11 120.79 ± 0.09 87.51 ± 0.48 42.08 ± 0.23
2 wt BIOC 163.29 ± 0.16 120.87 ± 0.18 88.88 ± 0.58 43.39 ± 0.29
0.5 wt% HEM 159.69 ± 0.08 117.64 ± 0.35 86.58 ± 1.92 41.63 ± 0.92
2 wt% HEM 160.87 ± 0.30 120.46 ± 0.23 95.25 ± 0.75 46.50 ± 0.37
0.5 wt% ROCH 160.48 ± 1.54 121.12 ± 0.15 76.14 ± 0.85 36.61 ± 0.41
2 wt% ROCH 160.72 ± 0.11 119.36 ± 0.04 81.46 ± 2.02 39.77 ± 0.99