Abstract
Graphitic carbon nitride (g-C3N4) is a polymeric semiconductor that has garnered considerable attention in photocatalysis due to its high activity in processes such as the degradation of organic pollutants, water splitting, and CO2 reduction. Tungsten trioxide (WO3), a metal oxide semiconductor known for its electrochromic, photochromic, and photocatalytic properties, has shown strong potential for coupling with g-C3N4 to enhance visible-light-driven photocatalytic performance. This study investigates the effect of varying WO3 content (0%, 3%, 5%, 7%, 9%) on the structural and photocatalytic properties of WO3@ g-C3N4 composites for Rhodamine B (RhB) degradation under visible light irradiation. The composites were synthesized via a hydrothermal method and characterized using XRD, FTIR, SEM, TEM, DRS, and PL analyses to evaluate their crystal structure, chemical bonding, surface morphology, band gap energy, and charge carrier dynamics. The results show that increasing WO3 content modifies the band structure and enhances charge separation efficiency. Photocatalytic tests demonstrated a progressive increase in RhB degradation efficiency with higher WO3 content, reaching a maximum of 99.7% after 210 min at 9% loading. The catalytic activity was only slightly affected by pH and the presence of reactive species scavengers. The enhanced performance of the 9% WO3@g-C3N4 composite is attributed to improved visible light absorption and reduced electron–hole recombination.


1. Introduction
The rapid deterioration of water quality caused by persistent organic pollutants, including various industrial dyes such as Rhodamine B (RhB), Crystal Violet (CV), Rose Bengal (RB), Safranin O (SO), Methylene Blue (MB), Eriochrome Black T (EBT), Acid Orange 7 (AO7), and Eosin Y (EY), has become a major global concern. These dyes are extensively used in the textile industry and pose serious environmental and health risks due to their colored pigments, nonbiodegradability, high toxicity, and potential carcinogenicity. Therefore, careful treatment of dye-containing wastewater is essential to prevent disadvantageous impacts on ecosystems and human health. ,
Various techniques have been developed for wastewater treatment, including physical (e.g., adsorption, membrane separation), chemical (e.g., ion exchange, oxidation, catalytic degradation), and biological approaches. Despite their widespread application, many of these conventional methods face significant challenges related to cost-effectiveness, treatment efficiency, and environmental impact. Among the emerging technologies, photocatalysis stands out as a promising alternative owing to its low cost, environmental compatibility, and high efficiency. − In this process, a photocatalyst absorbs light energy, generating reactive species capable of initiating redox reactions that convert dye pollutants into less toxic or benign substances. ,
The performance of photocatalysts in degrading organic pollutants depends heavily on their physicochemical properties and structural composition. Numerous studies have focused on the development of effective photocatalysts, such as titanium dioxide (TiO2), − zinc oxide (ZnO), − other metal oxide semiconductors, − and carbon-based nanomaterials. , Each of these materials exhibits unique advantages and limitations. Among them, graphitic carbon nitride (g-C3N4) − has emerged as a particularly potential photocatalyst, primarily beacause of its ease of synthesis via thermal polymerization of nitrogen-rich precursors (e.g., urea or melamine), additionally its favorable characteristics, including chemical stability, low toxicity, biocompatibility, and abundant availability. However, the photocatalytic performance of pristine g-C3N4 is hindered by several inherent limitations. These include limited absorption in the visible light spectrum and rapid recombination of photogenerated electron–hole pairs. Additionally, its moderate oxidation potential is sufficient only for water oxidation, lacking the ability to generate highly reactive hydroxyl radicals, which are necessary for nonselective degradation of organic pollutants. , Numerous modification techniques, including element doping, surface engineering, and heterojunction formation with other semiconductors, have been employed to enhance its photocatalytic activity. Notable examples of such hybrid systems include g-C3N4-based composites with TiO2, ZnO, SnO2, and DyVO4.
Tungsten trioxide (WO3) is considered a potential photocatalyst for organic dyes treatment because of its visible-light responsiveness with the band gap of 2.6–2.8 eV, high valence band position (∼3.1 eV), notable electron mobility (∼6.5 cm2/V·s), and excellent stability in acidic media. , However, the relatively low conduction band potential of pure WO3 (+0.5 V vs NHE at pH 0) limits its ability to produce superoxide radicals and causes rapid recombination of photogenerated charge carriers, thereby impairing overall photocatalytic performance. To overcome these drawbacks, the construction of a heterojunction with graphitic carbon nitride (g-C3N4) has proven effective in enhancing photocatalytic activity. In addition to expanding the spectrum of light absorption, the composition of WO3 and g-C3N4 enhances the solar energy utilization. Especially, the formation of a Z-scheme heterojunction between the two materials enables more efficient separation of electrons and holes, reducing recombination and enhancing redox reactions. , Additionally, WO3 contributes to the structural integrity and photocatalytic stability of the g-C3N4-based system during repeated use.
Numerous studies have demonstrated the effectiveness of WO3@g-C3N4 composites for degrading organic dyes such as Rhodamine B (RhB), with performance largely influenced by synthesis techniques and operating conditions. For instance, a study by Cui et al. (2016) reported nearly complete degradation of RhB using a 0.25 WO3@g-C3N4 composite under visible-light illumination from a 500 W source. Similarly, Yang et al. (2017) achieved approximately 90% RhB removal using a composite with 1 wt % WO3 content. Zhao et al. (2022) employed a ball-milling strategy to improve the composite’s surface area and interfacial contact, resulting in a degradation efficiency of 95.5%. In another case, Zheng et al. (2022) synthesized a 5 wt % WO3@g-C3N4 material that achieved 92% RhB degradation within 1 h, while also exhibiting enhanced activity through a photo-Fenton mechanism due to synergistic effects between photocatalysis and oxidizing agents. Despite these promising results, most studies have focused on narrow WO3 content ranges, and often lack systematic investigations into the roles of key environmental and reaction parameters such as catalyst dosage, solution pH, and reactive species.
To address these limitations, this study presents a comprehensive investigation of WO3@g-C3N4 nanocomposites with systematically varied WO3 content (0%, 3%, 5%, 7%, and 9%). The structural, morphological, and optical properties of the composites were thoroughly characterized, and their photocatalytic activities for RhB degradation under visible light were evaluated. Moreover, the effects of catalyst dosage, pH, and reactive species were examined in detail. Radical scavenger experiments and kinetic modeling were employed to elucidate the degradation mechanism and determine the relative contributions of different reactive species (e–, h+, ·OH, O2·–). This study not only identifies the optimal WO3 loading for maximum efficiency but also provides mechanistic insights into the charge transfer processes that govern the enhanced photocatalytic activity. The findings offer valuable guidance for designing advanced visible-light-driven photocatalysts for practical wastewater treatment applications.
2. Materials and Methods
Rhodamine B (RhB), 1,4-benzoquinone, and sodium tungstate (Na2WO4) were purchased from Sigma-Aldrich, while Xilong Scientific provided the sodium hydroxide (NaOH), hydrochloric acid (HCl), nitric acid (HNO3), sodium chloride (NaCl), Rhodamine B (RhB). For all experimental techniques, the solvent was deionized water from an Aquatron A4000D purification system. No additional purification was necessary because all analytical-grade reagents were used precisely as supplied. Analytical-grade reagents were all used exactly as supplied, requiring no further purification (Figure ).
1.
Schematic illustration of the synthesis procedure of WO3@g-C3N4 nanocomposite.
2.1. Sample Preparation
The WO3@g-C3N4 nanocomposite samples were designated as CN (pure g-C3N4), 3WCN, 5WCN, 7WCN, and 9WCN, corresponding to WO3 mass ratios of 0%, 3%, 5%, 7%, and 9%, respectively. The calculated amounts of chemicals used for the synthesis of each sample are summarized in Table .
1. Chemical Quantities Used for the Synthesis of WO3@g-C3N4 Composites.
| No. | Sample | WO3Weight Percentage (%) | m(g-C3N4) (g) | m′ (Na2WO4·2H2O) (g) | V(HNO3) (ml) |
|---|---|---|---|---|---|
| 1 | 0WCN | 0 | 1.200 | 0 | 0 |
| 2 | 3WCN | 3 | 1.164 | 0.066 | 0.36 |
| 3 | 5WCN | 5 | 1.140 | 0.099 | 0.54 |
| 4 | 7WCN | 7 | 1.116 | 0.132 | 0.72 |
| 5 | 9WCN | 9 | 1.092 | 0.165 | 0.90 |
2.2. Analytical Methods
The crystalline properties of the samples were examined by X-ray diffraction (XRD) using an X’Pert Pro MPD (PANalytical) instrument with CuK-α1 radiation (λ = 1.54056 Å), scanned at a rate of 0.03°/2s over a 2θ range of 10° to 80°. The chemical bonding on the sample surface was investigated by Fourier-transform infrared spectroscopy (FTIR) using a JASCO FT/IR-4600 type A, in the wavenumber range of 500–4000 cm–1. The surface morphology of the WO3@ g-C3N4 (WCN) nanocomposite was characterized using scanning electron microscopy (SEM), while detailed nanostructures were observed by transmission electron microscopy (TEM) using a JEM-1010 instrument. UV–vis diffuse reflectance spectra were recorded using a JASCO V-750 spectrophotometer in the wavelength range of 200–800 nm. Photoluminescence (PL) spectra were obtained using a Spectra-Hub1 spectrometer in the range of 370–700 nm.
2.3. Photocatalytic Activity Evaluation
To assess the WO3@g-C3N4 nanocomposite’s photocatalytic efficacy, 20 mg of the sample was dissolved in 50 mL of Rhodamine B (RhB) solution (10 ppm) in a 100 mL beaker. The suspension was stirred at 700 rpm under the irradiation of a 150 W LED lamp (High Bay light 150 W, SH-HB2–200W, λ ≥ 450 nm, China). At regular intervals of 30 min, 5 mL of the reaction mixture was collected and analyzed for RhB concentration using a UV–vis spectrophotometer. The photocatalytic degradation efficiency (H%) was calculated using the following equation:
| 1 |
where C 0 and C t (mg/L or ppm) are the initial and time-dependent concentrations of RhB, respectively, and I 0 and I t represent the absorbance intensities of the characteristic RhB peak at 554 nm at the initial time and at time t, respectively.
3. Results and Discussion
3.1. Characterization
The X-ray diffraction (XRD) patterns of the samples are presented in Figure a. In all cases, characteristic diffraction peaks of g-C3N4 are observed, notably at a 2θ angle of 26.2°, which is associated with the (002) plane and is explained by the interlayer stacking of aromatic conjugated systems. In addition to the characteristic peak of g-C3N4, the samples 3WCN, 5WCN, 7WCN, and 9WCN also exhibit distinct diffraction peaks corresponding to the orthorhombic phase of WO3·H2O. These peaks appear at 2θ angles of 16.5°, 25.6°, 34.9°, and 48.9°, which are indexed to the (100), (110), (020), and (220) planes, respectively, as reported in standard reference data. These peaks begin to emerge in the 3WCN sample and show increasing intensity with higher WO3 content. At the same time, the intensity of the (002) diffraction peak at 2θ ≈ 26.2° associated with g-C3N4 tends to decrease as the WO3 content increases. Notably, when the doping amount of WO3 reaches 9 wt.%, the (002) peak exhibits a slight shift, which may be attributed to the structural influence of the orthorhombic WO3·H2O phase. These observations confirm the successful formation of the WCN nanocomposite.
2.
(a) XRD patterns and (b) Fourier-transform infrared (FTIR) spectra of the WCN nanocomposite samples.
The information on the chemical bonds and characteristic functional groups of both the pure and composite samples was examined using Fourier-transform infrared (FTIR) spectroscopy, as shown in Figure b. All the nanocomposite samples exhibited similar spectral profiles, with absorption bands observed in the range of 1100–1750 cm–1. Strong peaks at approximately 1241, 1323, 1411, and 1461 cm–1 correspond to the stretching vibrations of C–N bonds within aromatic conjugated rings, while the stretching vibrations of C = N bonds are identified at 1569 and 1636 cm–1. In addition, a distinct and intense peak at 810 cm–1 is attributed to the bending vibrations of triazine units, indicating that the molecular structure of the synthesized g-C3N4 consists of triazine-based frameworks. Additionally, a wide absorption band in the 3000–3400 cm–1 range is attributed to the stretching vibrations of hydroxyl (−OH) or -NH groups from surface-adsorbed water molecules. These results suggest that the fundamental structure of g-C3N4 remains largely unchanged upon compositing with WO3, which is consistent with the XRD results.
To examine the surface morphology of the materials, SEM analysis was conducted on the synthesized samples, and the results are shown in Figure . The CN (g-C3N4) sample exhibits a layered morphology. Upon compositing with WO3, white clusters corresponding to WO3 particles appear on the CN surface. The number and distribution of these white clusters increase with higher WO3 content (Figure b–e). FESEM images of the 0WCN and 9WCN samples reveal that both materials maintain a layered structure. However, as shown in Figure b, the 9WCN sample exhibits a more porous texture compared to 0WCN. To confirm the presence of WO3 in the composite material, EDX analysis was performed on the 9WCN sample, specifically targeting the white clusters (Figure f). The elements W, C, N, and O are confirmed to be present in the sample by the EDX spectrum. Moreover, no unexpected elements were detected, indicating that the synthesized WCN composite possesses high purity.
3.
Scanning electron microscopy (SEM) images of the samples: (a) CN, (b) 3WCN, (c) 5WCN, (d) 7WCN, (e) 9WCN, and (f) EDX spectrum of 9WCN.
To further analyze the surface morphology of the composites, transmission electron microscopy (TEM) images of the CN and 9WCN samples were obtained and are shown in Figure . The CN sample exhibits an uneven, layered structure with an irregular morphology. In contrast, the 9WCN sample shows the presence of small, dispersed particles, which are attributed to the incorporation of WO3 into the g-C3N4 matrix.
4.
Transmission electron microscopy (TEM) images of the samples (a) CN and (b) 9WCN.
Figure shows the UV–vis reflectance spectra of the WCN samples. It is evident that as the WO3 doping ratio increases, the absorption peak shifts to longer wavelengths, thereby broadening the light absorption range. The absorption maxima are found in the range of 350–450 nm.
5.
(a) UV–vis diffuse reflectance spectra and (b) corresponding optical bandgap plots of the samples.
From the diffuse reflectance spectra of the WCN composite samples, the optical band gap (Eg) was determined using the Kubelka–Munk method. The optical band gap is calculated using the following formula:
| 2 |
where F(R) = (1 – R)2/2R is the reflectance function, which is obtained from the diffuse reflectance coefficient R; n is an exponent that changes based on the kind of electronic transition (n = 1/2, 2, 3/2, or 3 for direct allowed, indirect allowed, direct forbidden, or indirect forbidden transitions, respectively); hv is the incident photon’s energy; A is a constant; and E g is the optical band gap.
The calculation results are plotted as (F(R)hv)1/2 vs hv. The results show that the optical band gap of the pure CN sample is 2.70 eV, while the composite samples exhibit an increase in the band gap compared to the pure sample, with values of 2.73, 2.75, 2.72, and 2.74 eV for the 3WCN, 5WCN, 7WCN, and 9WCN samples, respectively. Thus, the optical band gap undergoes a shift with the incorporation of WO3 into the composite material.
Figure displays the PL spectra of pristine g-C3N4 (CN) and WO3@g-C3N4 composites with varying WO3 content (3–9 wt %). All samples exhibit a broad emission peak centered at ∼450 nm, commonly associated with the radiative recombination of photogenerated electron–hole pairs and intrinsic structural defects within g-C3N4. −
6.

PL spectra of g-C3N4 and WO3@g-C3N4 composite
As the WO3 content increases from 0 to 7 wt %, the PL intensity gradually rises, which is attributed to the formation of defect states or radiative recombination centers at the WO3@g-C3N4 interface. These defect-induced pathways enhance PL emission but reflect higher recombination rates, rather than improved charge separation.
At 9 wt % WO3 the PL intensity decreases, suggesting that a more effective charge transfer process may occur through the heterojunction, partially suppressing recombination. This implies a dual role of WO3: promoting radiative recombination at lower contents and enhancing charge separation at higher contents.
3.2. Investigation of Rhodamine B Degradation Performance
3.2.1. Effect of WO3 Loading Ratio
The photocatalytic degradation of Rhodamine B (RhB) was investigated using a series of WCN composite samples containing varying WO3 contents of 0%, 3%, 5%, 7%, 9%, and 11%, corresponding to the samples 0WCN (g-C3N4), 3WCN, 5WCN, 7WCN, 9WCN, 11WCN and WO3, respectively. The experiments were conducted under illumination with a 150 W LED lamp for a total duration of 210 min.
At the wavelength of 554 nm, an absorption peak corresponding to Rhodamine B (RhB) is observed. This absorption peak gradually decreases over time, indicating a reduction in RhB concentration within the solution. Furthermore, as the reaction time increases, a shift in the RhB absorption peak is noted, accompanied by a visible color change from pink to colorless. This phenomenon is attributed to the stepwise degradation of RhB into intermediate products during the photocatalytic process with the WCN composite samples.
The radar chart in Figure b clearly demonstrates the differences in photocatalytic performance among pristine WO3, g-C3N4(0WCN), and their composites at different ratios. Pure g-C3N4 (0WCN) exhibited a relatively removal medium efficiency (70.1%) and reaction rate constant (k = 0.91 × 10–2 min–1), while pure WO3 showed poor activity (k = 0.29 × 10–2 min–1, removal 49.6%). These results indicate that both components individually suffer from intrinsic drawbacks: WO3 is limited by narrow light absorption and fast e–- h+ recombination, whereas g-C3N4, despite its visible-light response, possesses low catalytic activity.
7.
(a) RhB absorption over time with CN and (b) effect of WO3 content on reaction rate and degradation efficiency.
With the incorporation of WO3, the photocatalytic activity was significantly enhanced owing to the formation of WO3 - g-C3N4 heterojunctions, where WO3 served as an efficient electron acceptor to improve charge separation and transfer. The 5WCN and 7WCN samples exhibited much higher rate constants (k = 1.44 and 1.82 × 10–2 min–1, with removal efficiencies of 98.4% and 99.0%, respectively), indicating the synergistic effect between WO3 and g-C3N4. The optimal performance was achieved with 9WCN (k = 1.95 × 10–2 min–1, 99.3% removal), suggesting that this ratio provided the best balance between light harvesting, charge separation, and available active sites. However, excessive WO3 loading (11WCN) led to reduced performance (k = 0.88 × 10–2 min–1, 96.5% removal), likely due to shielding effects and increased recombination. These findings are consistent with previous reports showing that WO3/g-C3N4 heterojunctions can broaden visible-light absorption and facilitate charge carrier separation more efficiently than either component alone. , Thus, optimizing WO3 loading is crucial for achieving superior photocatalytic activity in g-C3N4-based composites.
3.2.2. Effect of Catalyst Dosage and pH Conditions
After 9WCN was shown to be the best photocatalyst, more research was done to determine how different catalyst dosages (20 mg, 40 mg, 50 mg, 60 mg, and 80 mg) affected the photocatalytic degradation of Rhodamine B (RhB) during 210 min of 150 W LED irradiation. The findings are shown in Figure a, which shows the RhB UV–vis absorption spectra over time for various 9WCN sample doses. The degradation of RhB was also investigated at different pH values (pH 3, 5, 8, 9, and 10) under the same lighting settings to evaluate the impact of pH on photocatalytic efficiency. Figure b. illustrates the time-dependent UV–vis absorption spectra of RhB at different pH values, highlighting the impact of pH on the degradation performance of the 9WCN photocatalyst.
8.

Effect of (a) dosage and (b) pH on the reaction rate and photocatalytic efficiency.
Figure a illustrates the influence of varying 9WCN catalyst dosages on the reaction rate constant (k) and Rhodamine B (RhB) degradation efficiency. As the catalyst dosage increased from 20 mg to 60 mg, both k and the degradation efficiency exhibited an upward trend. Specifically, increasing the dosage from 20 mg to 40 mg resulted in a slight enhancement in reaction rate (k ≈ 0.0175 min–1), while the degradation efficiency rose from 97.6% to 99.0%. At 50 mg, the reaction rate increased more significantly to k = 0.0243 min–1. The 60 mg sample exhibited the highest performance, achieving the maximum reaction rate (k = 0.0307 min–1) and near-complete degradation efficiency (99.8%), confirming this as the optimal condition for photocatalytic performance. However, further increasing the catalyst dosage to 80 mg resulted in a slight decline in both parameters (k = 0.0297 min–1), likely due to light scattering and surface saturation effects, which limit effective contact between the catalyst and the RhB molecules.
These results suggest that increasing the amount of 9WCN catalyst from 20 mg to 60 mg enhances the number of active sites, thus improving photocatalytic activity. However, beyond 60 mg, the degradation efficiency reaches a plateau, and additional catalyst does not lead to a proportional increase in performance. Hence, the 60 mg dosage is identified as the optimal catalyst amount, delivering both the highest reaction rate and degradation efficiency.
Figure b presents the dependence of the reaction rate and degradation efficiency on the pH of the reaction medium. The degradation of RhB was least efficient in highly acidic (pH 3) and highly alkaline (pH 10) conditions, with corresponding rate constants of k = 0.0168 min–1 and k = 0.0162 min–1, respectively. In contrast, in near-neutral and mildly alkaline conditions, the catalyst exhibited significantly higher activity. At pH 6, the reaction rate reached k = 0.0184 min–1 with a degradation efficiency of 98.1%. A similar performance was observed at pH 9, with k = 0.0183 min–1 and 98.4% degradation. Notably, at pH 8, the catalyst achieved its highest photocatalytic activity, with k = 0.0203 min–1 and a degradation efficiency of 99.0%.
These results differ from some previous studies, which commonly report optimal degradation in strongly acidic or alkaline conditions. − However, findings by Yuan W. et al. (2017) also reported that RhB degradation efficiency could reach nearly 90% under near-neutral conditions (pH 7.1). This suggests that although the initial reaction rate in mildly alkaline conditions may be slower than in acidic environments, the overall degradation process is more complete over time under such conditions.
In summary, the 9WCN photocatalyst demonstrated excellent degradation efficiency across a wide pH range (pH 3–10), consistently exceeding 90%. These results highlight the material’s strong potential for practical wastewater treatment applications under varying environmental conditions.
3.2.3. Effect of Reactive Species
The photocatalytic activity of the 9WCN material was evaluated through the degradation of Rhodamine B (RhB) under 150 W LED illumination for 210 min in the presence of various scavengers, specifically hydrogen peroxide (H2O2), sodium oxalate (Na2C2O4), isopropanol (IPA), and benzoquinone (BQ). To elucidate the roles of the active species involved in the photocatalytic process, a series of control experiments were conducted using specific scavengers. In particular, H2O2 was employed as an electron scavenger, IPA was used as a specific scavenger for hydroxyl radicals (·OH), while Na2C2O4 and BQ were applied to capture superoxide radicals (·O2 –).
Figure illustrates the influence of various scavengers on the reaction rate constant (k) and the photocatalytic degradation efficiency of Rhodamine B (RhB) using the 9WCN catalyst. According to the figure, the addition of electrons (e–) and hydroxyl radical (·OH) scavengers, specifically H2O2 and IPA, resulted in a degradation efficiency of approximately 99.5%. This suggests that electrons and ·OH radicals do not play a dominant role in the photocatalytic degradation mechanism of RhB. These findings are consistent with previous studies investigating the effects of different scavengers. −
9.

Impact of various scavengers on photocatalytic efficiency and reaction rate.
In contrast, when hole (h+) and superoxide radical (O2·–) scavengers, such as sodium oxalate (Na2C2O4) and benzoquinone (BQ), were introduced, the degradation efficiency slightly decreased to 96.7% and 96.5%, respectively. This indicates that holes and superoxide radicals are involved in the degradation process, although they are not the primary reactive species. −
The trapping experiments revealed that, in the absence of scavengers, the reaction rate constant was k = 0.0307 min–1. Upon the introduction of specific scavengers, the rate constant decreased, confirming the contribution of each reactive species to the photocatalytic degradation process. The degree of contribution was further evaluated by calculating the inhibition ratio of each reactive species (e–, h+, ·OH, O2·–) based on the following formula:
| 3 |
where R x represents the inhibition ratio, k is the reaction rate constant in the absence of scavengers, and k scavenger is the rate constant in the presence of a specific scavenger.
For each reactive species, the corresponding inhibition ratios were 23.0%, 17.7%, 39.7%, and 66.2% for electrons (e–), holes (h+), hydroxyl radicals (·OH), and superoxide radicals (O2·–). These findings imply that holes (h+) and superoxide radicals (O2·–) are the primary factors influencing the photocatalytic degradation of RhB in the WO3@ g-C3N4 system, and that they are the most important components of the degradation process.
3.3. Mechanism of RhB Degradation by WO3@g-C3N4 Photocatalyst
In the WO3@g-C3N4 composite photocatalyst system, WO3 primarily acts as a visible-light-responsive material, initiating the generation of electron–hole pairs, while g-C3N4 serves as an effective electron acceptor. This heterojunction structure inhibits the recombination of photogenerated carriers and enables effective charge separation. Electrons from the conduction band (CB) of g-C3N4 are moved to the CB of WO3 upon light stimulation. In addition, because of their greater oxidative potential, the holes (h+) that are still present in the valence band of WO3 encourage the production of reactive hydroxyl radicals (·OH). ,
The production of hydroxyl and superoxide (O2·–) radicals, which are essential for the oxidative breakdown of RhB, is increased by this charge transfer pathway. The photocatalytic degradation of RhB involves a sequence of reactions, including N-deethylation, xanthene ring opening, and cleavage of aromatic structures, ultimately leading to the mineralization of the dye into simple inorganic species such as CO2, H2O, NO3 –, Cl–, and SO4 2–. Schematic Illustration of the Rhodamine B Degradation Mechanism shown in Figure .
10.
Schematic illustration of the rhodamine B degradation mechanism
4. Conclusions
In this study, WO3@g-C3N4 composites were synthesized via a hydrothermal method, and the influence of WO3 content on their photocatalytic performance was systematically investigated. The composite with 9 wt.% WO3 (9WCN) exhibited the highest Rhodamine B degradation efficiency (99.7%) under visible light, attributed to improved light absorption and effective charge separation at the heterojunction interface. Scavenger and parameter variation experiments confirmed that holes (h+) and superoxide radicals (O2·–) were the dominant reactive species. These findings demonstrate the strong potential of WO3@g-C3N4 for visible-light-driven wastewater treatment. Future work should focus on catalyst recyclability and performance under scaled-up conditions to support practical implementation.
Supplementary Material
Acknowledgments
This research is funded by Hanoi University of Civil Engineering (HUCE) under grant number 20-2024/KHXD-TĐ.
The Supporting Information is available free of charge at https://pubs.acs.org/doi/10.1021/acsomega.5c04874.
Additional structural characterization (XRD and FTIR spectra); morphological analysis (SEM, TEM, and EDX elemental mapping); optical properties (UV–Vis diffuse reflectance and photoluminescence spectra); effects of WO3 loading ratio, catalyst dosage and pH, reactive species trapping experiments (PDF)
The authors declare no competing financial interest.
References
- Rafiq A.. et al. Photocatalytic degradation of dyes using semiconductor photocatalysts to clean industrial water pollution. Journal of Industrial and Engineering Chemistry. 2021;97:111–128. doi: 10.1016/j.jiec.2021.02.017. [DOI] [Google Scholar]
- Brown M. A., De Vito S. C.. Predicting azo dye toxicity. Critical Reviews in Environmental Science and Technology. 1993;23(3):249–324. doi: 10.1080/10643389309388453. [DOI] [Google Scholar]
- Katheresan V., Kansedo J., Lau S. Y.. Efficiency of various recent wastewater dye removal methods: A review. Journal of Environmental Chemical Engineering. 2018;6(4):4676–4697. doi: 10.1016/j.jece.2018.06.060. [DOI] [Google Scholar]
- Shanker U., Rani M., Jassal V.. Degradation of hazardous organic dyes in water by nanomaterials. Environmental Chemistry Letters. 2017;15(4):623–642. doi: 10.1007/s10311-017-0650-2. [DOI] [Google Scholar]
- Khan W. U., Ahmed S., Dhoble Y., Madhav S.. A critical review of hazardous waste generation from textile industries and associated ecological impacts. Journal of the Indian Chemical Society. 2023;100(1):100829. doi: 10.1016/j.jics.2022.100829. [DOI] [Google Scholar]
- Gupta V. K., Suhas N.. Application of low-cost adsorbents for dye removal – A review. Journal of Environmental Management. 2009;90(8):2313–2342. doi: 10.1016/j.jenvman.2008.11.017. [DOI] [PubMed] [Google Scholar]
- Khan M. M., Pradhan D., Sohn Y.. Nanocomposites for visible light-induced photocatalysis. 2017 doi: 10.1007/978-3-319-62446-4. [DOI] [Google Scholar]
- Zhou R.. Preparation of photocatalyst, reaction mechanism and its application in environmental control. Highlights in Science Engineering and Technology. 2022;26:461–468. doi: 10.54097/hset.v26i.4027. [DOI] [Google Scholar]
- Wang L., Yu J.. Principles of photocatalysis. Interface science and technology. 2023;35:1–52. doi: 10.1016/B978-0-443-18786-5.00002-0. [DOI] [Google Scholar]
- Nakata K., Fujishima A.. TiO2 photocatalysis: Design and applications. Journal of Photochemistry and Photobiology C Photochemistry Reviews. 2012;13(3):169–189. doi: 10.1016/j.jphotochemrev.2012.06.001. [DOI] [Google Scholar]
- Guo Q., Zhou C., Ma Z., Yang X.. Fundamentals of TIO2 Photocatalysis: Concepts, mechanisms, and challenges. Adv. Mater. 2019;31(50):1901997. doi: 10.1002/adma.201901997. [DOI] [PubMed] [Google Scholar]
- Schneider J.. et al. Understanding TIO2Photocatalysis: Mechanisms and materials. Chem. Rev. 2014;114(19):9919–9986. doi: 10.1021/cr5001892. [DOI] [PubMed] [Google Scholar]
- Ong W.-J.. et al. Graphitic Carbon Nitride (g-C3N4)-Based Photocatalysts for artificial photosynthesis and environmental remediation: Are we a step closer to achieving sustainability? Chem. Rev. 2016;116(12):7159–7329. doi: 10.1021/acs.chemrev.6b00075. [DOI] [PubMed] [Google Scholar]
- Wen J., Xie J., Chen X., Li X.. A review on g-C 3 N 4 -based photocatalysts. Appl. Surf. Sci. 2017;391:72–123. doi: 10.1016/j.apsusc.2016.07.030. [DOI] [Google Scholar]
- Fu J., Yu J., Jiang C., Cheng B.. G-C3N4-Based heterostructured photocatalysts. Adv. Energy Mater. 2018;8(3):1701503. doi: 10.1002/aenm.201701503. [DOI] [Google Scholar]
- Wang J., Wang G., Wei X., Liu G., Li J.. ZnO nanoparticles implanted in TiO2 macrochannels as an effective direct Z-scheme heterojunction photocatalyst for degradation of RhB. Appl. Surf. Sci. 2018;456:666–675. doi: 10.1016/j.apsusc.2018.06.182. [DOI] [Google Scholar]
- Lops C.. et al. Sonophotocatalytic degradation mechanisms of Rhodamine B dye via radicals generation by micro- and nano-particles of ZnO. Applied Catalysis B Environment and Energy. 2019;243:629–640. doi: 10.1016/j.apcatb.2018.10.078. [DOI] [PMC free article] [PubMed] [Google Scholar]
- Woan K.. et al. Photocatalytic Carbon-Nanotube–TiO2 composites. Adv. Mater. 2009;21(21):2233–2239. doi: 10.1002/adma.200802738. [DOI] [Google Scholar]
- Al Kausor M., Chakrabortty D.. Graphene oxide based semiconductor photocatalysts for degradation of organic dye in waste water: A review on fabrication, performance enhancement and challenges. Inorg. Chem. Commun. 2021;129:108630. doi: 10.1016/j.inoche.2021.108630. [DOI] [Google Scholar]
- Madima N., Mishra S. B., Inamuddin I., Mishra A. K.. Carbon-based nanomaterials for remediation of organic and inorganic pollutants from wastewater. A review. Environmental Chemistry Letters. 2020;18(4):1169–1191. doi: 10.1007/s10311-020-01001-0. [DOI] [Google Scholar]
- Lu X., Wang Q., Cui D.. Preparation and photocatalytic properties of g-C3N4/TiO2 hybrid composite. Journal of Material Science and Technology. 2010;26(10):925–930. doi: 10.1016/S1005-0302(10)60149-1. [DOI] [Google Scholar]
- He Y.. et al. Synthesis, Characterization, and Activity Evaluation of DyVO4/g-C3N4 Composites under Visible-Light Irradiation. Ind. Eng. Chem. Res. 2012;51(45):14729–14737. doi: 10.1021/ie301774e. [DOI] [Google Scholar]
- Liu W., Wang M., Xu C., Chen S.. Facile synthesis of g-C3N4/ZnO composite with enhanced visible light photooxidation and photoreduction properties. Chemical Engineering Journal. 2012;209:386–393. doi: 10.1016/j.cej.2012.08.033. [DOI] [Google Scholar]
- Van K. N.. et al. Facile construction of S-scheme SnO2/g-C3N4 photocatalyst for improved photoactivity. Chemosphere. 2022;289:133120. doi: 10.1016/j.chemosphere.2021.133120. [DOI] [PubMed] [Google Scholar]
- Peleyeju M. G., Viljoen E. L.. WO3-based catalysts for photocatalytic and photoelectrocatalytic removal of organic pollutants from water – A review. Journal of Water Process Engineering. 2021;40:101930. doi: 10.1016/j.jwpe.2021.101930. [DOI] [Google Scholar]
- Dutta V.. et al. An overview on WO3 based photocatalyst for environmental remediation. Journal of Environmental Chemical Engineering. 2021;9(1):105018. doi: 10.1016/j.jece.2020.105018. [DOI] [Google Scholar]
- Chen S., Hu Y., Jiang X., Meng S., Fu X.. Fabrication and characterization of novel Z-scheme photocatalyst WO3/g-C3N4 with high efficient visible light photocatalytic activity. Mater. Chem. Phys. 2015;149–150:512–521. doi: 10.1016/j.matchemphys.2014.11.001. [DOI] [Google Scholar]
- Chen S., Hu Y., Meng S., Fu X.. Study on the separation mechanisms of photogenerated electrons and holes for composite photocatalysts g-C3N4-WO3 . Applied Catalysis B Environment and Energy. 2014;150–151:564–573. doi: 10.1016/j.apcatb.2013.12.053. [DOI] [Google Scholar]
- Liu X.. et al. Synergy of adsorption and visible-light photocatalytic degradation of methylene blue by a bifunctional Z-scheme heterojunction of WO3/g-C3N4 . Appl. Surf. Sci. 2017;405:359–371. doi: 10.1016/j.apsusc.2017.02.025. [DOI] [Google Scholar]
- Cui L.. et al. Facile preparation of Z-scheme WO3/g-C3N4 composite photocatalyst with enhanced photocatalytic performance under visible light. Appl. Surf. Sci. 2017;391:202–210. doi: 10.1016/j.apsusc.2016.07.055. [DOI] [Google Scholar]
- Wang P.. et al. Fabrication of WO3@g-C3N4 with core@shell nanostructure for enhanced photocatalytic degradation activity under visible light. Appl. Surf. Sci. 2017;423:197–204. doi: 10.1016/j.apsusc.2017.06.127. [DOI] [Google Scholar]
- Zhao Q.. et al. Facile ball-milling synthesis of WO3/g-C3N4 heterojunction for photocatalytic degradation of Rhodamine B. Chem. Phys. Lett. 2022;805:139908. doi: 10.1016/j.cplett.2022.139908. [DOI] [Google Scholar]
- Zheng J.. Highly efficient photocatalysis and photo Fenton-Like catalyst degradation of tetracycline and rhodamine B using novel porous Z-Scheme WO3/g-C3N4 of in situ synthesis. Crystal Research and Technology. 2022;57(12):2200135. doi: 10.1002/crat.202200135. [DOI] [Google Scholar]
- Luu Thi L. A.. et al. In Situ g-C3N4@ZnO Nanocomposite: One-Pot Hydrothermal Synthesis and Photocatalytic Performance under Visible Light Irradiation. Adv. Mater. Sci. Eng. 2021;2021:17–20. doi: 10.1155/2021/6651633. [DOI] [Google Scholar]
- Ho W. O.. et al. The Crystal Structure of Tungsttte, WO3-H2O. Can. Mineral. 1984;22:681–688. [Google Scholar]
- Cuong L. M.. et al. Kinetics and Adsorption Model of Methylene Blue on g-C3N4@WO3.H2O Nanoplate Composite. Int. J. Nanosci. 2021;20(5):1–10. doi: 10.1142/S0219581X21500459. [DOI] [Google Scholar]
- Wang X.. Preparation of heterojunction C3N4/WO3 photocatalyst for degradation of microplastics in water. Chemosphere. 2023;337:139206. doi: 10.1016/j.chemosphere.2023.139206. [DOI] [PubMed] [Google Scholar]
- Chen S., Hu Y., Meng S., Fu X.. Study on the separation mechanisms of photogenerated electrons and holes for composite photocatalysts g-C3N4-WO3 . Applied Catalysis B Environment and Energy. 2014;150–151:564–573. doi: 10.1016/j.apcatb.2013.12.053. [DOI] [Google Scholar]
- Li W.. et al. Evidence for the active species involved in the photodegradation process of methyl orange on TiO2 . J. Phys. Chem. C. 2012;116(5):3552–3560. doi: 10.1021/jp209661d. [DOI] [Google Scholar]
- Lin Y.. et al. Highly efficient photocatalytic degradation of organic pollutants by PANI-Modified TiO2 composite. J. Phys. Chem. C. 2012;116(9):5764–5772. doi: 10.1021/jp211222w. [DOI] [Google Scholar]
- Shi W.. et al. pH-controlled mechanism of photocatalytic RhB degradation over g-C3N4 under sunlight irradiation. Photochemical & Photobiological Sciences. 2021;20(2):303–313. doi: 10.1007/s43630-021-00019-9. [DOI] [PubMed] [Google Scholar]
- Liang F., Zhang Y.-H., He B., Yang J., Shi Q., Shi F.-N.. Enhanced photocatalytic degradation of imidacloprid and RhB by the precursor derived Bi12.7Co0.3O19.35 under different pH value. J. Phys. Chem. Solids. 2022;164:110638. doi: 10.1016/j.jpcs.2022.110638. [DOI] [Google Scholar]
- Hong J., Yuan N., Wang Y., Qi S.. Efficient degradation of Rhodamine B in microwave-H2O2 system at alkaline pH. Chemical Engineering Journal. 2012;191:364–368. doi: 10.1016/j.cej.2012.03.032. [DOI] [Google Scholar]
- Cui H.-J., Huang H.-Z., Yuan B., Fu M.-L.. Decolorization of RhB dye by manganese oxides: effect of crystal type and solution pH. Geochemical Transactions. 2015;16(1):10. doi: 10.1186/s12932-015-0024-2. [DOI] [PMC free article] [PubMed] [Google Scholar]
- Yuan W., Zhang C., Wei H., Wang Q., Li K.. In situ synthesis and immobilization of a Cu(II)–pyridyl complex on silica microspheres as a novel Fenton-like catalyst for RhB degradation at near-neutral pH. RSC Adv. 2017;7(37):22825–22835. doi: 10.1039/C7RA02916K. [DOI] [Google Scholar]
- Tomar R., Abdala A. A., Chaudhary R. G., Singh N. B.. Photocatalytic degradation of dyes by nanomaterials. Materials Today Proceedings. 2020;29:967–973. doi: 10.1016/j.matpr.2020.04.144. [DOI] [Google Scholar]
- Yadav S.. et al. A review on degradation of organic dyes by using metal oxide semiconductors. Environmental Science and Pollution Research. 2023;30(28):71912–71932. doi: 10.1007/s11356-022-20818-6. [DOI] [PubMed] [Google Scholar]
- Nagajyothi P. C., Vattikuti S. V. P., Devarayapalli K. C., Yoo K., Shim J., Sreekanth T. V. M.. Green synthesis: Photocatalytic degradation of textile dyes using metal and metal oxide nanoparticles-latest trends and advancements. Critical Reviews in Environmental Science and Technology. 2020;50(24):2617–2723. doi: 10.1080/10643389.2019.1705103. [DOI] [Google Scholar]
- Karimi-Nazarabad M., Goharshadi E. K.. Highly efficient photocatalytic and photoelectrocatalytic activity of solar light driven WO3/g-C3N4 nanocomposite. Sol. Energy Mater. Sol. Cells. 2017;160:484–493. doi: 10.1016/j.solmat.2016.11.005. [DOI] [Google Scholar]
- Wu P., Wang J., Zhao J., Guo L., Osterloh F. E.. Structure defects in g-C3N4 limit visible light driven hydrogen evolution and photovoltage. Journal of Materials Chemistry A. 2014;2(47):20338–20344. doi: 10.1039/C4TA04100C. [DOI] [Google Scholar]
- Huang S., Long Y., Ruan S., Zeng Y.-J.. Enhanced photocatalytic CO2 reduction in Defect-Engineered Z-Scheme WO3–X/G-C3N4 heterostructures. ACS Omega. 2019;4(13):15593–15599. doi: 10.1021/acsomega.9b01969. [DOI] [PMC free article] [PubMed] [Google Scholar]
- Shang H.. Boosting Photocatalytic N2 Fixation on N-Defect g-C3N4/WO3: the Synergistic Effects of Nitrogen Vacancy and Z-Scheme Heterojunction. Advanced Materials Technologies. 2023;8(5):2201579. doi: 10.1002/admt.202201579. [DOI] [Google Scholar]
Associated Data
This section collects any data citations, data availability statements, or supplementary materials included in this article.