In the original publication [1], there was an overlap in Figure 10 as published. The corrected Figure 10 appears below. The authors state that the scientific conclusions are unaffected. This correction was approved by the Academic Editor. The original publication has also been updated.
Figure 10.
SEM images of the laminated structure in the thickness direction of the prepared high-strength laminated bamboo composite: (a) radial section of raw bamboo; (b–j) radial section of samples 1 to 9.
Footnotes
Disclaimer/Publisher’s Note: The statements, opinions and data contained in all publications are solely those of the individual author(s) and contributor(s) and not of MDPI and/or the editor(s). MDPI and/or the editor(s) disclaim responsibility for any injury to people or property resulting from any ideas, methods, instructions or products referred to in the content.
Reference
- 1.Colince L., Qian J., Zhang J., Wu C., Yu L. Study on the Molding Factors of Preparing High-Strength Laminated Bamboo Composites. Materials. 2024;17:2042. doi: 10.3390/ma17092042. [DOI] [PMC free article] [PubMed] [Google Scholar]