1.
Bangul, K., Bilawal, K., Syed, B. A., Waseem, U. K., Junchen, L., Shohidul, I., Iyapan, G., Raffi U. S. A., Mohamed E. H., Bee L. K. Ion‐Driven Interfacial Engineering of MXene‐PAM Hydrogels for Advanced Wearable ECG and AI‐Driven Blood Pressure Monitoring. Small Science. 2026; 6: e202500526. https://doi.org/10.1002/smsc.2025005264
In the originally published version of this article, a notation error appeared in the y‐axis labels of the strain‐dependent resistance change graphs. Specifically, the relative resistance change was incorrectly labeled as ΔR/R instead of the correct notation ΔR/R 0. This error occurred in the following figures: Figure 5 in the main manuscript and Supporting Figures 13, 14, and 15 in the Supporting Information. The figures have now been corrected to display the accurate notation ΔR/R 0. This correction does not affect any data, results, or conclusions presented in the article.
FIGURE 5.

Strain performance characterization of PAM, PAM–CaCl2, and ion‐driven Ti3C2T x –PAM hydrogel. (A) Relative resistance changes (ΔR/R 0) in ion‐driven Ti3C2T x –PAM hydrogel over a strain range from 300 to 1000%. (B) Gauge factors and relative resistance changes (ΔR/R 0) in ion‐driven Ti3C2T x –PAM hydrogel at 400 to 1000% strains. (C) Response and recovery times for the ion‐driven Ti3C2T x –PAM hydrogel at 25% strain. (D) Stability characterization through relative resistance variations (ΔR/R 0) in ions‐driven Ti3C2T x –PAM hydrogel when stretched to 100%, across 1000 consecutive cycles. (E) Stability characterization through relative resistance variations (ΔR/R 0) in ion‐driven Ti3C2T x –PAM hydrogel when stretched to 100%, 300%, 500%, 800%, and 1000% strain across 100 consecutive cycles. (F) Conductivity measurements for hydrogel samples: S‐1 (PAM + 0.5M CaCl2 + MX 0.5%), S‐2 (PAM + 0.5M CaCl2 + MX 1%), and S‐3 (PAM + 0.5M CaCl2 + MX 1.5%). Error bars represent mean ± SD (n = 3). (G) Real‐time monitoring of relative resistance changes (ΔR/R 0) in ion‐driven Ti3C2T x –PAM hydrogel during finger bending at various angles. (H) Real‐time monitoring of relative resistance changes (ΔR/R 0) in ion‐driven Ti3C2T x –PAM hydrogel during elbow bending at various angles. (I) Real‐time relative resistance changes (ΔR/R 0) in ion‐driven Ti3C2T x –PAM hydrogel are monitored during wrist bending at various angles.
Supporting Figure 13.

Relative resistance changes (ΔR/R 0) in Ions‐driven Ti3C2Tx–PAM hydrogel over a 10–300% strain range.
Supporting Figure 14.

Gauge factors and relative resistance changes (ΔR/R 0) in Ions‐driven Ti3C2Tx–PAM hydrogel at 10 to 300% strains.
Supporting Figure 15.

Relative resistance changes (ΔR/R 0) in Ions‐driven Ti3C2Tx–PAM hydrogel over a 100% strain range at −20°C, 0°C and 40°C.
We apologize for this error.