Oscillatory rheology dynamic frequency sweep measurements of 2 wt% MAX1 and 1 wt% MAX8 hydrogels, 25 mM HEPES, DMEM at pH 7.4, 37 °C. (G′ = storage modulus, G″ = loss modulus). Strain = 0.2%, gap height = 0.5 mm.