Skip to main content
. Author manuscript; available in PMC: 2010 Jul 21.
Published in final edited form as: Nano. 2009;4(1):1–5. doi: 10.1142/S1793292009001447

Fig. 3.

Fig. 3

SEM images of containers with approximately 63 nm sized pores, constructed by templating 750 nm PS particles. SEM image of (a) the top view (which forms the inside of the faces of the container after self-assembly) of the 2D cruciform after Ni electrodeposition, and (b) of a single face with (c)–(d) progressively zoomed-in detail of the region marked in (b). SEM image of (e) a nanoporous container after assembly and (f)–(h) progressively zoomed-in detail of the outer face of the container.