Figure 2

Bending responses as a function of time for microcantilevers coated by HRP prepared using methods A and B on exposure to 1 × 10−5 M H2O2 solution. For each method, three independent microcantilevers were tested. Only one test from method A was shown for clarity. The standard error was within 10%.