J Conserv Dent. 2013 Sep;16(5):462-5.
Comparative evaluation of push-out bond strength of ProRoot MTA, Biodentine, and MTA Plus in furcation perforation repair.
The line in discussion “The blood-contaminated MTA samples had a push-out bond strength of 4.8 ± 0.56 MPa and 9.2 ± 0.72 MPa at 24 h and 7 days respectively”.
Should be read as
“The blood-contaminated MTA samples had a push-out bond strength of 4.8 ± 0.56 MPa and 8.2 ± 0.72 MPa at 24 h and 7 days respectively”.
The error is regretted
- Editor, JCD