Figure 4.

Figure 4

(A) Surface roughness of PA-YK-NO coatings exposed to shear stress. (B) The lateral force required to remove coatings exposed to shear stress. (C) Depth of PA-YK-NO coating before and after shear stress. In all three cases, there is no difference compared to controls.