Skip to main content
. 2012 Oct;3(4):323–333. doi: 10.1177/1947603512447301

Figure. 2.

Figure. 2.

Hemispherical impactor tip geometry (A) and a representative Pressurex pressure-sensitive film impact pattern (B). (C) Footprints recorded with different sensitivity Pressurex pressure-sensitive films under equal loads (set to deliver 588 N [120 MPa] as described in Materials and Methods) delivered to rabbit condyles in situ were calibrated and parsed in 10% increments for load (MPa).