Abstract
The properties of ultraviolet (UV) photodetector fabricated on TiO2/diamond film were investigated. Single crystal diamond layer was grown on high-pressure-high-temperature Ib-type diamond substrate by microwave plasma chemical vapor deposition method, upon which TiO2 film was prepared directly using radio frequency magnetron sputtering technique in Ar and O2 mixing atmosphere. Tungsten was used as electrode material to fabricate metal-semiconductor-metal UV photodetector. The dark current is measured to be 1.12 pA at 30 V. The photo response of the device displays an obvious selectivity between UV and visible light, and the UV-to-visible rejection ratio can reach 2 orders of magnitude. Compared with that directly on diamond film, photodetector on TiO2/diamond film shows higher responsivity.
UV photodetector is becoming increasingly important for its special applications in industry, instrument and our daily life such as flame detection, environment security, information technology, medical treatment and inter-satellite communication1. Since a high-performance photodetector should satisfy the 5S requirements known as high sensitivity, high signal-to-noise ratio, high spectral selectivity, high speed and high stability2, traditional UV-enhanced Si photodetector has some limitations in UV detection, for its bandgap energy is only 1.1 eV, which brings high cost filters and high temperature sensitivity3. Thus researchers began to develop photodetectors on wide bandgap semiconductors such as GaN4, ZnO5, SiC6 and Ga2O37. Diamond also becomes an extraordinary candidate for ultraviolet photodetectors thanks to its wide band-gap, high carrier mobility, radiation hardness and thermal stability8. Earlier researches on diamond photodetector relied on natural diamonds, high-pressure high-temperature (HPHT) diamonds and polycrystalline diamonds. Recently, with the development of chemical vapor deposition (CVD) technique, high quality single crystal (SC) diamonds have been successfully grown onto low-cost diamond substrates9. And then, photodetectors with different structures on SC diamonds have been experiencing enthusiastic study, which shows highly desirable to satisfy the 5S requirements10,11. To realize a low dark current, as-grown diamond sample is oxidized to change the hydrogen termination surface into oxygen termination surface2. However, for undoped SC diamond epitaxial layer, the responsivity and UV-to-visible rejection ratio is relatively low when the surface is oxidized2.
TiO2 is another wide bandgap semiconductor, which is actively developed as detectors to be applied in the field of gas sensor, photocatalysis and solar cells12. Recently, TiO2 based photodetector has been fabricated by magnetron sputtering method, indicating very low dark current and high responsivity13,14. Thus, it is easy to think that combining TiO2 with diamond may provide a way to enhance the responsivity. Moreover, for a photodetector, when the photon energy is larger than the bandgap, the responsivity tends to decrease15. Considering that the bandgap of diamond is larger than that of TiO2, the combination of diamond and TiO2 may widen the spectral detecting range. This work is an attempt to deposit TiO2 directly on unintentionally doped SC diamond epitaxial layer to develop UV-photodetectors, whose optoelectronic characteristics have been investigated.
Results and Discussion
Figure 1(a) shows the Ramen spectrum of the homoepitaxial diamond layer. There is only a sharp peak at 1332 cm−1 with a full width at half maximum of 3.9 cm−1, indicating a high-quality diamond layer16. Figure 1(b) exhibits the SEM image of TiO2 film sputtered on diamond layer and some interspaces exist between crystal grains. The TiO2 film may be polycrystalline. It was reported that oxygen partial pressure is important for depositing TiO2 film, because it may influence plasma potential, discharge voltage, and deposit rate17. In our deposition process, the partial pressure ratio of Ar to O2 was set as 2:1.
Figure 2 shows the schematic of photodetectors. The photodetector based on TiO2/diamond film is denoted as Sample A, and the other fabricated on diamond film is named as Sample B which is used for comparison. Since the electron affinity of TiO2 is about 4.3 eV, tungsten (W) with a work function of 4.55 eV was selected as electrode material in sample A to form ohmic contact. As for sample B, Pd was used to form ohmic contact. Dark currents of sample A and sample B were investigated and shown in Fig. 3. Both I–V curves are almost linear, showing that W/TiO2 and Pd/diamond contacts are both ohmic contacts. The dark current of sample A was measured to be 0.5 pA at bias voltage of 4 V. When the bias voltage increased to 30 V, the dark current increased slowly to 1.12 pA. For sample B, the dark currents are 1.28 pA and 1.9 pA at 4 V and 30 V, respectively. Both detectors show extremely low dark current, which plays an important role in lowering the signal to noise ratio18. Moreover, the dark currents are comparable, indicating that TiO2 film on diamond may not introduce additional leakage current path.
The photocurrents of sample A and sample B were investigated by using UV-light with the parameter of 180 nW/mm2 at 220 nm and 23 μW/mm2 at 340 nm, as shown in Fig. 4. Compared to dark currents shown in Fig. 3, it indicates a significant increase of photocurrent in Fig. 4. For both detectors, photocurrents increase with bias voltage increasing, and no saturation phenomenon appears even at 30 V. A possible reason is that the electric field is not strong enough to collect all the photo-generated carriers before their recombination. Under the illumination of both 340 nm and 220 nm, the photocurrents of sample A are bigger than that of sample B, indicating a higher photo response of TiO2/diamond detector.
Figure 5 shows the responsivity of sample A varying with the wavelength changing under different bias voltages. The photo responsivity shows a decrease tendency with wavelength increasing. An obvious rejection ratio between UV and visible light can be observed. When the bias voltage is 10 V, under the illumination of 220 nm, 340 nm and 400 nm, the responsivity of sample A detector is calculated to be 0.071 A/W, 0.013 A/W and 0.00071 × 10−4A/W, respectively. Thus, the UV-to-visible rejection ratios for 340 nm versus 400 nm and 220 nm versus 400 nm are 18 and 100, respectively. When the bias voltage is increased to 30 V, the responsivity is evaluated to be 0.2 A/W, 0.048 A/W and 0.0019 A/W, leading to rejection ratios of 25 and 105, respectively. This indicates that when the bias voltage increases, the responsivity and rejection ratio also increase. The phenomenon is in agreement with the unsaturation of photocurrent. When higher electric field is applied, more photo-generated carriers can be collected, leading to responsivity enhancement. The detectivities of Sample A at 220 nm and 340 nm are 6.57 × 1010/W and 1.33 × 1010/W, respectively, indicating good UV detective ability.
Figure 6 shows the spectral response of both detectors at 30 V, which displays the difference between TiO2/diamond detector (sample A) and diamond detector (sample B). For sample B, when the bias voltage is 30 V, under the illumination of 220 nm, 340 nm and 400 nm, the responsivity is calculated to be 0.13 A/W, 0.02 A/W and 0.0019 A/W, respectively. The UV-to-visible rejection ratio for 340 nm versus 400 nm is 11, while that for 220 nm versus 400 nm is 68. Compared to sample A, both of the responsivity and rejection ratio are lower. This means that the structure of TiO2/diamond can enhance the detector responsivity and rejection ratio.
In order to investigate if sample A is depended on only TiO2 film, typical spectral responses of TiO2 detectors reported in references 13 and 19 are used for comparison. In reference 13, the highest responsivity is at a light wavelength of 250 nm, and the responsivity decreases when the wavelength is above or less than 250 nm. In reference 19, the highest responsivity is at 340 nm, and the responsivity tends to decrease when light wavelength becomes shorter. However, the spectral response of sample A detector is different, in which responsivity increases with the wavelength ranging from 400 nm to 220 nm. This phenomenon could be attributed to the TiO2/diamond joint film structure. When TiO2 is deposited on diamond, a gradient energy band would form in the interface, as shown in Fig. 7(a). When the incident UV light wavelength is shorter than cut-off wavelength, electrons can jump from the valence band to the conduction band. When the light wavelength is 360 nm, corresponding to the cut-off wavelength of TiO2, electron-hole pairs are generated in TiO2 film, as shown in Fig. 7(b). Then the carriers shift along the electrode field, and are collected by the electrodes. When the light wavelength is between 225 nm and 360 nm, the electron-hole pairs are generated both in interface and TiO2, as shown in Fig. 7(c), leading to an increase of photocurrent. When the light wavelength is shorter than 225 nm, which corresponds to the cut-off wavelength of diamond, electron-hole pairs are generated in TiO2, interface, and diamond, as shown in Fig. 7(d). Thus, more carriers contribute to photocurrent, resulting in a higher photo responsivity. For traditional TiO2 photodetector, it is fabricated only on TiO2 film is used as the works. Even though the light wavelength becomes shorter than cut-off wavelength, the amount of carriers remain the same, making no effect on improving the responsivity. In contrast, the responsivity may decrease, as shown in references 13 and 19.
Figure 8 shows the transient response of Sample A and Sample B under the illumination pulse of 248 nm light. The light pulse is generated by a KrF excimer laser, with a frequency of 20 Hz and a duration time of 50 ns. The insert show the increasing time of the photodetector. For Sample A, the increasing time is about 20 μs, and the decreasing time is about 1000 μs, as shown in Fig. 8(a). For Sample B, the increasing time is about 2 μs, and the decreasing time is about 400 μs, as shown in Fig. 8(b). For both photodetectors, the decreasing time is much longer than the increasing time, which is attributed to the delay in the decay of the photo-generated carrier density16. Compared to Sample B, the response time of Sample A is longer. The mechanisms could be considered as: one is that the oxygen molecules adsorption and desorption process on the TiO2 surface leads to the a slow response speed20; another is that the defects in the TiO2 film hinder the collection of some photo-generated carriers, leading to a longer response time21.
Conclusions
In summary, the properties of ultraviolet photodetector fabricated on TiO2/diamond film have been investigated. TiO2 film has been directly deposited on single crystal diamond epitaxial layer by radio frequency magnetron technique. W electrodes were patterned on TiO2/diamond film to fabricate UV photodetector. This device exhibits 1.12 pA dark current at 30 V, and shows 2 orders of magnitude UV-to-visible rejection ratio. Compared with that of TiO2 photodetector, this device indicates increasing responsivity in a wide light wavelength range, which could be attributed to the gradient energy band structure in the interface of TiO2/diamond film. Also, the device shows higher responsivity than that on diamond. Transient response shows that the increasing time of the device is 20 μs and the decreasing time is 1000 μs.
Methods
About 2 μm undoped SC diamond epitaxial layer was grown on 3 × 3 × 0.3 mm3 Ib-type HPHT diamond substrate by microwave plasma chemical vapor deposition method. The total flow rate of H2 and CH4, the ratio of CH4/(H2+CH4), the process pressure, the growth temperature and the microwave power were 500 sccm, 0.8%, 80 Torr, 850 °C and 800 W, respectively. Raman spectrum was used to characterize the quality of the epitaxial layer. After growth, the sample was boiled in acid mixture (H2SO4:HNO3 = 1:1 by volume) at 300 °C for 2 h to change the hydrogen terminated surface to oxygenated surface.
Half of this epitaxial layer was used to deposit TiO2 by radio frequency magnetron sputtering technique. The source material was 3 inches sintered TiO2 ceramic target with the purity of 99.99%. The background pressure was as low as 3 × 10−4 Pa. Ar and O2 were used as sputtering gas, whose flow rate were 40 sccm and 20 sccm, respectively. Before deposition, the target was cleaned by Ar ion for five minutes. During sputtering process, the power was 150 W, and the working pressure was 1.2 Pa. The thickness of TiO2 was measured to be 450 nm. Another half of diamond layer remained as oxygenated surface state.
Two W electrodes with a thickness of 100 nm were patterned on TiO2/diamond film using radio frequency magnetron sputtering method to fabricate the novel photodetector. The electrode width was 1000 μm and the space between electrodes was 200 μm. Thus the total active area was 0.2 mm2. Two Pd electrodes with a thickness of 50 nm were patterned on diamond film using thermal evaporation method to fabricate traditional diamond photodetector. These two electrodes had the same parameters as W electrodes. The I–V characteristics of the as-fabricated photodetectors were investigated by Agilent B1505A power device analyzer. The optoelectronic properties were evaluated with a Keithley 6487 picoammeter/voltage source, a 500 W Xe lamp source and a monochromator. The light power at the sample surface was measured by a commercial UV-enhanced Si detector. The time response is measured by a KrF excimer laser and an oscilloscope.
Additional Information
How to cite this article: Liu, Z. et al. Fabrication of UV Photodetector on TiO2/Diamond Film. Sci. Rep. 5, 14420; doi: 10.1038/srep14420 (2015).
Acknowledgments
This work was supported by the Ministry of Science and Technology (Grant No. 2013AA03A101) of China.
Footnotes
Author Contributions Z.C.L. and H.X.W. performed the design of the device. Z.C.L. and F.L. performed the device fabrication. Z.C.L and F.N.L. performed the measurements. S.Y.L., C.H., F.W. and W.W. performed the data analysis. Z.C.L. write this manuscript and all authors participate in discussions.
References
- Sang L. W., Liao M. Y. & Sumia S. A comprehensive review of semiconductor ultraviolet photodetectors: From thin film to one-dimensional nanostructures. Sensors. 13, 10482–10518 (2013). [DOI] [PMC free article] [PubMed] [Google Scholar]
- Liao M. Y. et al. Comprehensive investigation of single crystal diamond deep-ultraviolet detectors. Jpn. J. Appl. Phys. 51, 090115 (2012). [Google Scholar]
- Lou Y. Y. et al. CVD diamond detector for ultraviolet radiation. Functional Materials. 35, 442–446 (2004). [Google Scholar]
- Chung S. J. et al. Optical absorption and anomalous photoconductivity in undoped n-type GaN. Appl. Phys. Lett. 76, 1021–1023 (2000). [Google Scholar]
- Law J. B. K. & Thong J. T. L. Simple fabrication of a ZnO nanowire photodetector with a fast photoresponse time Appl. Phys. Lett. 88, 133114 (2006). [Google Scholar]
- Chen X. P., Zhu H. L., Cai J. F. & Wu Z. Y. High-performance 4H-SiC-based ultraviolet p-i-n photodetector. J. Appl. Phys. 102, 024505 (2007). [Google Scholar]
- Weng W. Y. et al. A high-responsivity GaN nanowire UV photodetector. IEEE Journal of Selected Topics in QuantumElectronics. 17, 996–1001 (2011). [Google Scholar]
- Wang L. J., XiaY. B. & Ju J. H. The influence of the film’s microstructure on electrical properties of the CVD diamond X-ray detector. J. Infrared Millim. Waves. 21, 11–14 (2002). [Google Scholar]
- Balducci A., Marinelli M., Milani E. & Morgada M. E. Extreme ultraviolet single-crystal diamond detectors by chemical vapor deposition. Appl. Phys. Lett. 86, 193509 (2005). [Google Scholar]
- Liao M. Y., Alvarez J. & Koide Y. Single Schottky-barrier photodiode with interdigitated-finger geometry: Application to diamond. Appl. Phys. Lett. 90, 123507 (2007). [Google Scholar]
- Liao M. Y., Koide Y. & Alvarez J. Thermally stable visible-blind diamond photodiode using tungsten carbide Schottky contact. Appl. Phys. Lett. 87, 022105 (2005). [Google Scholar]
- Qi H. F. & Liu D. B. Effect of growth technology of TiO2 film on photoelectronic properties of TiO2 UV detector. Journal of Aeronautical Materials. 32, 47–50 (2012). [Google Scholar]
- Huang H. L. et al. Low-dark-current TiO2 MSM UV photodetectors with Pt Schottky Contacts. IEEE Electron Device Letters. 32, 530–532 (2011). [Google Scholar]
- Huang H. L. et al. Growth anf fabrication of sputtered TiO2 based ultraviolet detectors. Applied Surface Science 29, 248–254 (2014). [Google Scholar]
- Zhang X. A., Wu H., Zhang H. L., Wang F. & Jia H. W. Analysis on spectrum response pf silicon photoelectric diode. Physical Experiment of College. 24, 2 (2011). [Google Scholar]
- McKeag Robert D. et al. Polycrystalline diamond photoconductive device with high UV-visible discrimination. Appl. Phys. Lett. 67, 2117–2119 (1995). [Google Scholar]
- Domaradzki J. et al. Microstructure and optical properties of TiO2 thin films prepared by low pressure hot target reactive magnetron sputtering. Thin Solid films. 513, 269–274 (2006). [Google Scholar]
- Hao G. Q., Zhang Y. G., Liu T. D. & Li A. Z. The dark current characteristics of InGaAs PIN photodetectors. Semiconductor Optoelectronics. 25, 341–345 (2004). [Google Scholar]
- Xie Y. N. et al. Low dark current metal-semiconductor-metal ultraviolet photodetectors based on sol-gel-derived TiO2 films. Journal of Applied Physics. 109, 023114 (2011). [Google Scholar]
- Lu G. Q., Linsebigler A. Jr. & John T. Yates. The adsorption and photodesorption of oxygen on the TiO2 (110) surface. The Journal of Chemical Physics. 102, 4657 (1995). [Google Scholar]
- Tsai Tsung-Ying et al. A visible-blind TiO2 nanowire photodetector. Journal of the electrochemical society. 159, 4, J132–J135 (2012). [Google Scholar]