Figure 4.
(a) Water contact angle PEEK before and after 10 and 30 min of oxygen plasma treatment; (b) graph showing water contact angle with plasma treatment time for PEEK and PC; (c) bar graph showing the polar (σP) and dispersive (σD) component of the surface energy of the three polymers before and after plasma treatment calculated using Owens/Wendt theory.